美国杜邦 POM 107 物性
性能项目 | 测试条件 | 测试方法 | 数值/描述 | 单位 | ||
机械性能 | 拉伸强度(引张强度) | ASTM D638/ISO 527 | kg/cm²(MPa)[Lb/in2] | |||
断裂伸长率 | ASTM D638/ISO 527 | 3 | % | |||
拉伸模量 | ASTM D638/ISO 527 | 10000 | kg/cm²(MPa)[Lb/in2] | |||
拉伸屈服伸长率(延伸率) | ASTM D638/ISO 527 | % | ||||
拉伸断裂伸长率(延伸率) | ASTM D638/ISO 527 | 190 | % | |||
弯曲模量(弯曲弹性率) | ASTM D790/ISO 178 | kg·cm/cm(J/M)ft·lb/in | ||||
弯曲强度 | ASTM D790/ISO 178 | kg·cm/cm(J/M)ft·lb/in | ||||
洛氏硬度 | ASTM D785 | |||||
IZOD 缺口冲击强度 | 1/4" 23℃ | ASTM D256/ISO 179 | 80 | kg·cm/cm(J/M)ft·lb/in | ||
1/4" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||||
1/8" 23℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||||
1/8" -30℃ | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||||
Charpy冲击强度 | 23℃ (缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | |||
-30℃(缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||||
23℃(无缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||||
-30℃(无缺口) | ASTM D256/ISO 179 | kg·cm/cm(J/M)ft·lb/in | ||||
物性性能 | 比重(密度) | ASTM D792/ISO 1183 | 1.37 | |||
成型收缩率 | ASTM D955 | % | ||||
熔融指数(流动系数) | 200℃/5kg | ASTM D1238/ISO 1133 | g/10min | |||
220℃/10kg | ASTM D1238/ISO 1133 | g/10min | ||||
吸水率 23℃/24H | ASTM D570/ISO 62 | 0.8 | % | |||
热性能 | 热变形温度 | 退火 | ASTM D648/ISO 75 | 255 | ℃(℉) | |
未退火 | ASTM D648/ISO 75 | ℃(℉) | ||||
维卡软化点 | ASTM D1525/ISO R306 | ℃(℉) | ||||
熔点 | - | 255 | ℃(℉) | |||
燃烧性(率) | UL94 | HB | ||||
线性膨胀系数 | ASTM D696/ISO 11359 | 2.5 | mm/mm.℃ |
- 代理美国杜邦 耐摩擦POM 500CL 抗磨耗 适合耐磨损性 2024-11-22
- 美国杜邦 POM 500 中粘 抗冲击 抗蠕变 杜邦公司聚甲醛 2024-11-22
- 长期供应POM 美国杜邦 100 均聚甲醛 高粘度 Zui坚韧硬度 2024-11-22
- 超韧POM 美国杜邦 500T 低磨耗 适合超韧性工程制品 2024-11-22
- 美国杜邦POM原料 100ST 超强韧性 高粘度 齿轮应用 2024-11-22
- 代理美国杜邦POM 100T 超高韧性 2024-11-22
- Zytel PA612树脂 158L NC010 注坯模型 挤压级通用 2024-11-22
- Zytel杜邦尼龙 PA66 FE5382 BK276 33%玻璃纤维稳定的热挤压树脂 2024-11-22
- 杜邦Zytel 超级强韧尼龙66 ST801A 超级强韧 聚酰胺66树脂 2024-11-22
- Zytel 尼龙66 FE240012 BK010 高度挤压的变坚韧 2024-11-22